首頁 > 供應(yīng)產(chǎn)品 > 湖北 供應(yīng)都鑫F-20一次還原鐵粉
湖北 供應(yīng)都鑫F-20一次還原鐵粉
產(chǎn)品: 瀏覽次數(shù):1187湖北 供應(yīng)都鑫F-20一次還原鐵粉 
品牌: 都鑫
品牌: 都鑫
型號(hào): F-20
單價(jià): 2600.00元/噸
最小起訂量: 1 噸
供貨總量: 10000 噸
發(fā)貨期限: 自買家付款之日起 天內(nèi)發(fā)貨
有效期至: 長期有效
最后更新: 2021-11-14 02:01
 
詳細(xì)信息
品牌 都鑫
型號(hào) F-20
凈重 25000
顏色 黑色
保質(zhì)期(月) 6

   

還原鐵粉

是利用固體或氣體還原劑還原鐵的氧化物來制取海綿狀的鐵。還原過程中分為一次還原和二次還原。一次還原**是固體碳還原制取海綿鐵,一次還原主要流程是:鐵精礦→烘干→磁選→粉碎→篩分→裝罐→進(jìn)入一次還原爐→海綿鐵。二次精還原流程:海綿鐵→清刷→破碎→磁選→二次還原爐→粉塊→解碎→磁選→篩分→分級(jí)→混料→包裝→成品。用還原法所生產(chǎn)的**鐵粉,各項(xiàng)參數(shù)達(dá)標(biāo),F(xiàn)e≥98%,C≤0.01%,磷和硫都小于0.03%,氫損為0.1~0.2%。

我公司是采用軋鋼**鐵鱗經(jīng)二次氫氣還原制成海綿狀**鐵粉,技術(shù)指標(biāo)達(dá)到**標(biāo)準(zhǔn)規(guī)定。具有以下特點(diǎn):

高純度、低夾雜、一致性好、細(xì)粉含量高、壓縮性和成型性好。

在摩擦行業(yè)中:

一次還原鐵粉主要用于半金屬摩擦材料中和鋼釬維一起構(gòu)成其中的金屬部分;

二次還原鐵粉可使摩擦系數(shù)平穩(wěn),相對(duì)于一次還原鐵粉,它是少孔結(jié)構(gòu)有利于半金屬摩擦材料代鋼纖維主要組成部分,減少纖維用量。提高摩擦材料的制品性能。

Reduced iron powder

Through reductant iron utilization of solid or gas to produce sponge iron oxide. The first reduction and the second reduction take the part of the reduction process. The reduction of producing sponge iron is solid carbon reduction, its main process is: the iron concentrate, drying, magnetic separation, crushing, sieving, canning, into a reduction furnace, sponge iron. The second reduction process: sponge iron, cleaning, crushing, magnetic separation, the two reduction furnace, powder and solution of fragmentation, separation, screening, classification, mixing, packaging and finished product. Using high quality iron powder reduction method in the production of various parameters, standard, Fe ≥ 98%,C≤ 0.01%, phosphorus and sulfur both less than 0.03%, hydrogen loss ranged from 0.1 to 0.2%.

Our company is using high quality steel iron scale through two hydrogen reduction into cavernous quality iron powder, technical indicators have reached the national standard. characteristics following :

High purity, low inclusion, good consistency, high content of fine powder, compression and molding.

In friction industry:

The reduced iron powder is mainly used in semi-metallic friction material and steel fiber together constitute one of the metal parts;

The second reduced iron powder can make smooth friction coefficient, relative to a reduced iron powder, it is less porous structure facilitates the semi-metallic friction material steel fiber main part, improve product performance of friction materials.

產(chǎn)品技術(shù)指標(biāo) Technical Indices

項(xiàng)目Item

單位Unit

檢測(cè)結(jié)果Test   Result

比重 Density

g/cm3

5.0-5.8

固定鐵 Fixed Fe

%

85/95

**可溶物 Hydrochloric Acid Soluble

%

0.5/0.3

粒度 Size

mesh

80 & 100